A polyolefin having a density of greater than about 0.930 g/ml which when extruded at a temperature in the range of from about 590° F. to about 645° F. and then coated onto a substrate at a rate of from about 300 ft/min to about 1000 ft/min has an edge weave of from about 0 in/side to about 2.5 in/side and a neck-in of less than about 3.0 in/side.