Patent attributes
A salicide process is provided. A metal layer selected from a group consisting of titanium, cobalt, platinum, palladium and an alloy thereof is formed over a silicon layer. A first thermal process is performed. Next, a second thermal process is performed, wherein the second thermal process includes a first step performed at 600˜700 degrees centigrade for 10˜60 seconds and a second step performed at 750˜850 degrees centigrade for 10˜60 seconds. If the metal layer is selected from a group consisting of nickel and an alloy thereof is formed on a silicon layer, the first step of the second thermal process is performed at 300˜400 degrees centigrade for 10˜60 seconds and the second step of the second thermal process is performed at 450˜550 degrees centigrade for 10˜60 seconds.