Patent attributes
Systems and methods for low-manganese welding alloys are disclosed. An example arc welding consumable may comprise: between 0.4 and 1.0 wt % manganese; strengthening agents selected from the group consisting of nickel, cobalt, copper, carbon, molybdenum, chromium, vanadium, silicon, and boron; and grain control agents selected from the group consisting of niobium, tantalum, titanium, zirconium, and boron. The grain control agents may comprise greater than 0.06 wt % and less than 0.6 wt % of the welding consumable. The resulting weld deposit may comprise a tensile strength greater than or equal to 70 ksi, a yield strength greater than or equal to 58 ksi, a ductility (as measured by percent elongation) of at least 22%, and a Charpy V-notch toughness greater than or equal to 20 ft-lbs at −20° F. The welding consumable may provide a manganese fume generation rate less than 0.01 grams per minute during the arc welding operation.