Patent attributes
The present invention relates to a propylene polymer composition comprising a long chain branched propylene polymer, wherein said propylene polymer composition has a) a crystallization temperature Tc of less than 115° C., b) a melting temperature Tm of less than 155° C. c) a F30 melt strength of from 5.0 to less than 30.0 cN, and d) a V30 melting extensibility of more than 190 mm/s, a process for producing said propylene polymer composition by reactive modification of a propylene polymer in the presence of a peroxide, an article comprising said propylene polymer composition, the use of said propylene polymer composition for producing an article.