A method may include reprocessing a polymer composition comprising a crosslinked polymeric composition, wherein the crosslinked polymeric composition comprises a matrix polymer having a polar polymer internal phase that is selectively crosslinked with a crosslinking agent, wherein the reprocessed polymer composition retains an environmental stress cracking resistance within 60% of the value for the initial polymer composition when measured according to ASTM D-1693 procedure B and wherein the reprocessed polymer composition presents a Normalized Property Balance Index (NPBI) greater than about 1.0.