A method of making pre-sintered preforms using a mixture of base superalloy particles and titanium-containing boron and silicon free braze alloy particles, such as for the repair of superalloy gas turbine engine components. Alloy particles as large as 2 mm provide reduced shrinkage when compared to prior art preforms. Braze material compositions disclosed herein are boron and silicon free and may have melting temperature ranges as low as 10° C., and they include no element not already present in the composition of the superalloy component.