While a molten metal of copper heated to a temperature, which is higher than the melting point of copper by 250 to 700° C. (preferably 350 to 650° C. and more preferably 450 to 600° C.), is allowed to drop, a high-pressure water is sprayed onto the heated molten metal of copper in a non-oxidizing atmosphere (such as an atmosphere of nitrogen, argon, hydrogen or carbon monoxide) to rapidly cool and solidify the heated molten metal of copper to produce a copper powder which has an average particle diameter of 1 to 10 μm and a crystallite diameter Dx